Printers whose heated bed clears 100 °C. Essential for reliable ABS, ASA and PA-CF adhesion without lifting corners.
- #1
ANYCUBICKobra S1 MaxC$1171 CoreXY · heated chamber · 42.9 L · 350°C · LeviQ 3.0 - #2
FLSUNS1 DeltaC$999 Delta · 44.0 L · 350°C · Automatic - #3
ORIGINAL PRUSACORE OneC$2236 CoreXY · heated chamber · 14.8 L · 290°C · Load cell - #4
R QIDI TECHNOLOGYQIDI PLUS4C$799 CoreXY · 26.2 L · 370°C · Automatic - #5
snapmaker3 in 1 AddonsC$1134 · 56.0 L · 300°C - #6
R QIDI TECHNOLOGYQIDI Q2C$699 CoreXY · 18.7 L · 370°C · Loadcell Sensor - #7
CrealityK2 PlusC$1700 CoreXY · 42.9 L · 350°C · Strain gauge - #8
ANYCUBICKobra X Multi-Colour 4-Colour PrintingC$409 Bedslinger · 17.6 L · 300°C - #9
ELEGOOCentauri Carbon 2 CoreXY Build Volume 256×C$539 CoreXY · 16.8 L · 350°C · Full-Auto Calibration - #10
FLASHFORGEAdventurer 5MC$417 CoreXY · 10.6 L · 280°C · Automatic
No listings match your current marketplace selection - tick more sources above.
Matt's take
Bed temperature is the quiet spec that separates "can print ABS if you cross fingers" from "prints ABS reliably". Most PLA-focused machines top out at 70-80 °C because that is all PLA needs. ABS wants 100-110 °C, ASA similar, and filled nylons 90-110 °C. Without that bed heat, corners peel as the print cools and you end up running a brim or raft on every part. Pair with an active heated chamber for best results - bed heat alone helps but doesn't fully solve warp on tall ABS.
Frequently asked
Do I need a 100 °C heated bed? +
Only if you print ABS, ASA, or filled nylons. PLA and PETG are happy at 60-80 °C. If you never leave PLA territory, a high-temp bed is unused capability.
Why does bed temperature matter for ABS? +
ABS shrinks as it cools from its 100 °C+ print temperature. A hot bed keeps the bottom layers near glass transition, so the shrink happens gradually rather than snapping the print off the plate at hour three.
Is a garolite/FR4 bed surface different from PEI? +
Garolite is the de-facto surface for nylon because nylon refuses to stick to PEI. If you plan to print nylon, check that the printer either ships a garolite plate or accepts a swap-in one. Otherwise it is an extra £30 and often an extra week's wait.