Printers whose heated bed clears 100 °C. Essential for reliable ABS, ASA and PA-CF adhesion without lifting corners.
- #1
ANYCUBIC( Grey PLA) Anycubic Kobra S1 MAX + 6KG PL$765 CoreXY · heated chamber · 42.9 L · 350°C · LeviQ 3.0 - #2
CrealityK2 Plus$1003 CoreXY · heated chamber · 42.9 L · 350°C · Strain gauge - #3
R QIDI TECHNOLOGYQIDI Max4$1299 CoreXY · heated chamber · 51.7 L · 370°C · Loadcell Sensor Integrated int - #4
R QIDI TECHNOLOGYQIDI Plus5 Multi-Color$899 CoreXY · heated chamber · 30.7 L · 370°C · Loadcell - #5
FLASHFORGECreator 5 Pro Industrial$849 CoreXY · heated chamber · 16.8 L · 320°C · Fully Automatic Calibration & - #6
CrealityK1 Max$481 CoreXY · 27.0 L · 300°C · AI LiDAR - #7
CrealityK2 Plus$972 CoreXY · 42.9 L · 350°C · Strain gauge - #8
R QIDI TECHNOLOGYQIDI Q2C$349 CoreXY · 18.9 L · 370°C · Loadcell Sensor Integrated int - #9
ComgrowCreality K2 Plus Multi Color Printing$1199 CoreXY · 42.9 L · 350°C - #10
ANYCUBICChristmas Silk PLA 4KG + Anycubic Kobra S1$460 CoreXY · 15.6 L · 320°C · LeviQ3.0
No listings match your current marketplace selection - tick more sources above.
Matt's take
Bed temperature is the quiet spec that separates "can print ABS if you cross fingers" from "prints ABS reliably". Most PLA-focused machines top out at 70-80 °C because that is all PLA needs. ABS wants 100-110 °C, ASA similar, and filled nylons 90-110 °C. Without that bed heat, corners peel as the print cools and you end up running a brim or raft on every part. Pair with an active heated chamber for best results - bed heat alone helps but doesn't fully solve warp on tall ABS.
Frequently asked
Do I need a 100 °C heated bed? +
Only if you print ABS, ASA, or filled nylons. PLA and PETG are happy at 60-80 °C. If you never leave PLA territory, a high-temp bed is unused capability.
Why does bed temperature matter for ABS? +
ABS shrinks as it cools from its 100 °C+ print temperature. A hot bed keeps the bottom layers near glass transition, so the shrink happens gradually rather than snapping the print off the plate at hour three.
Is a garolite/FR4 bed surface different from PEI? +
Garolite is the de-facto surface for nylon because nylon refuses to stick to PEI. If you plan to print nylon, check that the printer either ships a garolite plate or accepts a swap-in one. Otherwise it is an extra £30 and often an extra week's wait.